Drying of sawn timber

Drying of sawn timber After sawing, timber must be dried to reach the moisture content required for each purpose of use. The drying grades applied to sawn timber are shipping dry and carpenter dry. The moisture content of shipping-dry timber must be 18–24 %, while that of carpenter-dry timber must be 8–14 %. When drying